Physical Modeling for Optimization of Process of Bottom Blowing Argon in a 100 t Ladle
更新时间:2026-01-21
    • Physical Modeling for Optimization of Process of Bottom Blowing Argon in a 100 t Ladle

    • Special Steel   Vol. 35, Issue 1, Pages: 11-14(2014)
    • Received:19 July 2013,

      Online First:05 September 2022,

      Published:05 September 2014

    移动端阅览

  • 田恩华, 李东侠, 崔衡, et al. Physical Modeling for Optimization of Process of Bottom Blowing Argon in a 100 t Ladle[J]. Special Steel, 2014, 35(1): 11-14. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

A Study on Water Model for Optimum Location of 150 t Ladle Bottom Blowing Argon Nozzle
Water Modeling Examination for Optimization of Bottom Argon Blowing Location in 250 t Ladle Refining
A Study on Water Modelling for Bottom Blowing Oxygen Stirring of a 100 kg Medium Frequency Induction Furnace
Numerical Simulation of Effect of 100 t Bottom-Blowing Argon Ladle with Immersed Cylinder on Liquid Flow Field
A Study on Water Model for Optimum Process of Bottom Blowing Argon of 120 t Ladle

Related Author

林路
包燕平
陈序
周俐
倪修华
张才贵
齐洪杰
李保卫

Related Institution

北京科技大学钢铁冶金新技术国家重点实验室
安徽工业大学冶金与资源学院
宝钢股份上海梅山钢铁股份有限公司技术中心
内蒙古科技大学,内蒙古自治区白云鄂博矿多金属资源综合利用重点实俭室: 省部共建国家重点实验室培养基地
辽宁科技大学材料与冶金学院
0