Equipment Characteristics and Practice of Continuous Casting Process for Large Round Bloom of Special Steels at Huaigang
更新时间:2026-01-21
    • Equipment Characteristics and Practice of Continuous Casting Process for Large Round Bloom of Special Steels at Huaigang

    • Special Steel   Vol. 34, Issue 4, Pages: 22-25(2013)
    • Received:22 February 2013,

      Online First:11 September 2022,

      Published:11 September 2013

    移动端阅览

  • 王忠英, 仝太钦, 刘兆方, et al. Equipment Characteristics and Practice of Continuous Casting Process for Large Round Bloom of Special Steels at Huaigang[J]. Special Steel, 2013, 34(4): 22-25. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Process Practice to Control of Precipitation of TiN in ER70S-G Welding Wire Steel Containing Titanium and Prevent Nozzle Clogging
Present Status and Development of Continuous Casting Technology for Special Steel in China
A Study on Distribution Characteristics of Electromagnetic Field in Concasting Mould for Round Bloom
Analysis on Clogging of Submerged Entry Nozzle for 409L Stainless Steel Concasting and Improved Measure
Process Practice for Production of Caterpillar Track Steel 35MnBM by 90    t    EAF-LF(VD)-CC-CR    Flow    Sheet

Related Author

杨咏阶
干勇
王忠英
郭上型
王建军
周俐
李卫国
施晓芳

Related Institution

青岛钢铁控股集团有限责任公司炼钢总厂
宝山钢铁股份有限公司不锈钢分公司
东北特钢集团北满特殊钢有限责任公司
北京科技大学冶金与生态工程学院
中咨工程建设监理公司总工办
0