Application of Limestone Used to Control End Temperature of Liquid in 120 t Top and Bottom Combined Blowing Converter
更新时间:2026-01-21
    • Application of Limestone Used to Control End Temperature of Liquid in 120 t Top and Bottom Combined Blowing Converter

    • Special Steel   Vol. 34, Issue 5, Pages: 44-46(2013)
    • Received:08 April 2013,

      Online First:22 September 2022,

      Published:22 September 2013

    移动端阅览

  • 解英明. Application of Limestone Used to Control End Temperature of Liquid in 120 t Top and Bottom Combined Blowing Converter[J]. Special Steel, 2013, 34(5): 44-46. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Analysis and Process Practice on Steelmaking Technology of 100 t Top-Blown Oxygen Converter by Limestone for Slag Making
Practice of Electro-Slag Remelting Process for 6.2 t Slab Ingot of High Nitrogen Dual-Phase Stainless Steel
Practice of Process for Production of Steel 14Cr1Mo by 30t EAF-LF-VD-13 t Casting Ingot Flowsheet

Related Author

秦登平
杨建平
危尚好
张建师
孙剑光
刘金旭
王新鹏
陈帅超

Related Institution

首秦金属材料有限公司
洛阳双瑞特种装备有限公司
兰州兰石能源装备工程研究院有限公司
甘肃省高端铸锻件工程技术研究中心
0