Experimental Study on Hot Deformation Behavior and Math Models for Deformation Resistance of EA4T Axle Steel for High Speed Rail
更新时间:2026-01-21
    • Experimental Study on Hot Deformation Behavior and Math Models for Deformation Resistance of EA4T Axle Steel for High Speed Rail

    • Special Steel   Vol. 34, Issue 3, Pages: 60-63(2013)
    • Received:18 December 2012,

      Online First:22 September 2022,

      Published:22 September 2013

    移动端阅览

  • 徐刚, 李士琦, 王乐, et al. Experimental Study on Hot Deformation Behavior and Math Models for Deformation Resistance of EA4T Axle Steel for High Speed Rail[J]. Special Steel, 2013, 34(3): 60-63. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Hot Rolling Parameters on Deformation Resistance of Coarse-Grained Niobium Steel
Hot Deformation Behavior of 2507 Super Duplex Stainless Steel
Development of Secondary Cooling Water Distribution Model for Large-Size Round Bloom Casting
A Study on Recrystallization of Fluoride Free Titanium Bearing Solidified Flux Film of Casting Powder in Mold
Study on Regularity of Temperature Reduction of IF Steel Slab Casting Liquid with 210 t Top and Bottom Combined Blown Converter-RH Flow Sheet

Related Author

刘清友
孙新军
文建华
雷霆
阴树标
花福安
刘丽丽
王佳夫

Related Institution

钢铁研究总院结构材料研究所
昆明理工大学材料与冶金工程学院
东北大学轧制技术及连轧自动化国家重点实验室
烟台宝钢钢管有限责任公司
中冶京诚工程技术有限公司
0