A Study on Water Modeling of an 150 t Ladle Bottom Argon Blowing
更新时间:2026-01-21
    • A Study on Water Modeling of an 150 t Ladle Bottom Argon Blowing

    • Special Steel   Vol. 34, Issue 3, Pages: 18-21(2013)
    • Received:17 December 2012,

      Online First:16 September 2022,

      Published:16 September 2013

    移动端阅览

  • 李文双, 朱荣, 鲍翔, et al. A Study on Water Modeling of an 150 t Ladle Bottom Argon Blowing[J]. Special Steel, 2013, 34(3): 18-21. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Physical Simulation of Inclusion Removal and Slag Entrapment in 210 t RH Refining Process
A Study on Water Model for Optimum Location of 150 t Ladle Bottom Blowing Argon Nozzle
Water Modeling Examination for Optimization of Bottom Argon Blowing Location in 250 t Ladle Refining
Numerical Simulation of Effect of 100 t Bottom-Blowing Argon Ladle with Immersed Cylinder on Liquid Flow Field
A Study on Water Model for Optimum Process of Bottom Blowing Argon of 120 t Ladle

Related Author

迟云广
沈巧珍
吴墨环
彭明耀
肖尊湖
陈序
包燕平
林路

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
华菱涟源钢铁有限公司
北京科技大学钢铁冶金新技术国家重点实验室
宝钢股份上海梅山钢铁股份有限公司技术中心
安徽工业大学冶金与资源学院
0