Effect of Adding Rare Earth Element La Alloying Process for Stainless Steel Fe-20Cr-5Al on Yield of La
更新时间:2026-01-21
    • Effect of Adding Rare Earth Element La Alloying Process for Stainless Steel Fe-20Cr-5Al on Yield of La

    • Special Steel   Vol. 35, Issue 3, Pages: 29-32(2014)
    • Received:18 December 2013,

      Online First:29 August 2022,

      Published:29 August 2014

    移动端阅览

  • 余晓艳, 刘建华, 杨波锋, et al. Effect of Adding Rare Earth Element La Alloying Process for Stainless Steel Fe-20Cr-5Al on Yield of La[J]. Special Steel, 2014, 35(3): 29-32. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Production Practice on Bottom Blowing Nitrogen Alloying during 30 t VOD Refining Process

Related Author

安杰
赵越
李忠伟
魏仁杰

Related Institution

抚顺特殊钢股份有限公司1技术处
第二炼钢厂
0