Characteristics of Hot Metal Pretreatment KR Desulphurized Sludge and Development of Recycling Technology of Resources
更新时间:2026-01-21
    • Characteristics of Hot Metal Pretreatment KR Desulphurized Sludge and Development of Recycling Technology of Resources

    • Special Steel   Vol. 34, Issue 6, Pages: 42-44(2013)
    • Received:19 June 2013,

      Online First:07 September 2022,

      Published:07 September 2013

    移动端阅览

  • 石枚梅, 俞海明. Characteristics of Hot Metal Pretreatment KR Desulphurized Sludge and Development of Recycling Technology of Resources[J]. Special Steel, 2013, 34(6): 42-44. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of KR Pretreatment Process Parameters on Hot Metal Desulphurization Results
Effect of Initial Silicon Content in Metal on Simultaneous Removal of Silicon, Manganese, Phosphorus and Sulphur during Metal Pretreatment Process
Analysis and Optimization on Hot Metal KR Desulphurization Process by Response Surface Methodology
Effect of Microscopic Structure of Lime on Desulphurization of Pretreated Hot Metal

Related Author

薛正良
高志强
曹维
徐绪林
王炜
李闯
郭汉杰
潘明旭

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
武汉钢铁集团公司
北京科技大学冶金与生态工程学院
大冶特殊钢股份有限公司炼钢事业部
高品质特殊钢湖北省重点实验室
0