Process Practice for Gear Steel 20CrMnTi Produced by 120 t BOF-LF-CC Flow Sheet
更新时间:2026-01-21
    • Process Practice for Gear Steel 20CrMnTi Produced by 120 t BOF-LF-CC Flow Sheet

    • Special Steel   Vol. 35, Issue 2, Pages: 40-42(2014)
    • Received:14 October 2013,

      Online First:09 September 2022,

      Published:09 September 2014

    移动端阅览

  • 丁礼权, 范植金, 罗国华, et al. Process Practice for Gear Steel 20CrMnTi Produced by 120 t BOF-LF-CC Flow Sheet[J]. Special Steel, 2014, 35(2): 40-42. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Process Practice for Microstructure Optimization of UNS N09925 Alloy Forgings in Oilfield Service Industry
The Effect of Nb on Microstructure and Properties of GH4169 Alloy Pipe
Microstructure and High-temperature Mechanical Properties of Different Positions of Turbine Disc Forgings in GH4706 Superalloy
Research on Ultra-high Rotary Bending Fatigue Strength of Flexible Bearing Steels for Robot Harmonic Speed Reducer
Effect of AlN and Zr Microalloying on Thermoplasticity and Grain Size of Carburized Gear Steel

Related Author

Zhang Jiawei
Yang Liang
Yu Jie
Wu Yinhu
Zhu Yuliang
Wang Shucai
Zhong Qiang
Liu Zhengdong

Related Institution

Central Iron & Steel Research Institute Co.,Ltd.
Fushun Special Steel Co.,Ltd.
China Iron & Steel Research Institute Group
Zhejiang Jiuli Metal Materials Research Institute Co., Ltd.
Zhejiang Jiuli Hi-Tech Metals Co., Ltd.
0