Process Practice for Improving Service Life of Submerged Nozzle in Mold by using Double-Slag-Line Operation
更新时间:2026-01-21
    • Process Practice for Improving Service Life of Submerged Nozzle in Mold by using Double-Slag-Line Operation

    • Special Steel   Vol. 35, Issue 6, Pages: 32-34(2014)
    • Received:30 June 2014,

      Online First:19 August 2022,

      Published:19 August 2014

    移动端阅览

  • 于学森, 沈奎, 廖舒纶, et al. Process Practice for Improving Service Life of Submerged Nozzle in Mold by using Double-Slag-Line Operation[J]. Special Steel, 2014, 35(6): 32-34. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Analysis on Clogging of Submerged Entry Nozzle for 409L Stainless Steel Concasting and Improved Measure
Development of Nb Microalloying High Speed Steel TGM2A-S for Taps
Numerical and Physical Simulation on Fluid Flow Field in Mold of Vertical Slab Caster
A Study on Water Model for Liquid Level Fluctuation and Impact Depth of Flow in Mold for Slab Casting
Control of Casting Slab Surface Longitudinal Cracks of 0.12%-0.16% C Chromium Molybdenum Steel

Related Author

陆斌
李实
王立江
陈旭
郑宏光
雷利军
仇圣桃
陈远清

Related Institution

宝山钢铁股份有限公司不锈钢分公司
江苏天工工具有限公司,丹阳
昆明理工大学冶金与能源工程学院
钢铁研究总院连铸技术国家工程研究中心
华菱涟源钢铁公司
0