Progress of Research on Interfacial Properties of Fluoride-Containing Slag System for Electroslag Remelting
更新时间:2026-01-21
    • Progress of Research on Interfacial Properties of Fluoride-Containing Slag System for Electroslag Remelting

    • Special Steel   Vol. 35, Issue 3, Pages: 19-23(2014)
    • Received:30 December 2013,

      Online First:27 August 2022,

      Published:27 August 2014

    移动端阅览

  • 曹玉龙, 姜周华. Progress of Research on Interfacial Properties of Fluoride-Containing Slag System for Electroslag Remelting[J]. Special Steel, 2014, 35(3): 19-23. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Surface Tension of Pentary Slag CaF2 -CaO-Al2O3 -SiO2 -MgO and Its Application in Nickel Base Alloy Electro-Slag Remelting
Effect of Slag Ingredient on Ti Burning Loss Rate and Ingot Surface Quality of High Temperature Alloy 0Cr15Ni25Ti2MoAlVB
Effect of Electromagnetic Stirring on Temperature Field of ESR Ingot
Control of Carbon and Sulfur Content in Electroslag Remelting Pure Iron
Progress of Research on Performance of Passive Films of Stainless Steels

Related Author

刘立
赵俊学
李献民
丁五洲
陈峰
李小孟
赵鸿燕
白海军

Related Institution

西安建筑科技大学
宝钛集团有限公司
太原钢铁(集团)公司技术中心
北京科技大学材料科学与工程学院
太钢不锈钢股份有限公司技术中心
0