Numerical Simulation of Solidification Process of 40CrNiMo Steel 35 t Polygonal Ingot
更新时间:2026-01-21
    • Numerical Simulation of Solidification Process of 40CrNiMo Steel 35 t Polygonal Ingot

    • Special Steel   Vol. 35, Issue 5, Pages: 26-29(2014)
    • Received:16 April 2014,

      Online First:01 September 2022,

      Published:01 September 2014

    移动端阅览

  • 李卫平, 钱国钢, 季克进, et al. Numerical Simulation of Solidification Process of 40CrNiMo Steel 35 t Polygonal Ingot[J]. Special Steel, 2014, 35(5): 26-29. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Numerical Simulation of 80 mm Extra-thick Plate Stacking Slow Cooling for EH420 Marine Steel
Numerical Simulation of Solidification Structure for 4J36 Invar Alloy Ingot
The Effect and Control of Rare Earth Ce on Carbonitrides Precipitation in 441 Ferritic Stainless Steel
Effect of Melting Rate on Solidification Process of High Filled Ratio 06Cr18Ni11Ti Electroslag Remelting Ingot
Thermodynamic Coupling Analysis of Air Cooling for X70 Pipeline Steel Continuous Casting Slab Based on ABAQUS

Related Author

Jiang Dongbin
Liu Zhaoxia
Liu Jun
Sun Xianjin
Yi Qing
Wu Xiaolin
Ren Ying
Zhang Lifeng

Related Institution

User Application Technology Research Institute, Citic Pacific Special Special Steel Group Co.,Ltd., Jiangyin
School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
Jiangyin Xingcheng Special Steel Works Co., Ltd., Jiangyin
School of Mechanical and Material Engineering, North China University of Technology
Technology Center of Baowu Special Metallurgy Co., Ltd.
0