Production Practice of Nb-Ti Microalloying and Containing Cr Steel J55 for Oil Casing Tube
更新时间:2026-01-21
    • Production Practice of Nb-Ti Microalloying and Containing Cr Steel J55 for Oil Casing Tube

    • Special Steel   Vol. 36, Issue 4, Pages: 28-30(2015)
    • Received:15 February 2015,

      Online First:25 August 2022,

      Published:25 August 2015

    移动端阅览

  • 吕国成, 包丽明, 朱金禄, et al. Production Practice of Nb-Ti Microalloying and Containing Cr Steel J55 for Oil Casing Tube[J]. Special Steel, 2015, 36(4): 28-30. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Controlled Rolling and Controlled Cooling and Cooling Bed Heat Preservation Process on Mechanical Properties of 42CrMo Steel φ50 mm Rolled Bar
Effects of Controlled Rolling and Controlled Cooling on Microstructure and Mechanical Properties of Low-Alloy Steel Q355D Heavy Plates
Influence of Phosphorus Microalloying on Molidification, Hot Deformation and Mechanical Properties in Nickel/Nickel Iron-based Alloys
Effect of Heat Treatment on Mechanical Properties of High Strength Free-Cutting Precipitation Hardening Stainless Steel 2Cr16Ni3Mo2CuN
Effect of Quenching and Tempering Process on Mechanical Properties of Spring Steel 60Si2CrVAT

Related Author

金启邦
孙世平
王青海
年国恩
鲜奋强
吕晓芳
孙伟
杜慧起

Related Institution

西宁特殊钢集团有限责任公司1精品小棒线分厂
股份公司
技术中心
邢台职业技术学院资源与环境工程系
2天津中德应用技术大学机械工程学院
0