Structure and Mechanical Properties of Welded Joint of ∅336 mm x 31 mm Pipe of Martensite Heat Resistant Steel P91
更新时间:2026-01-21
    • Structure and Mechanical Properties of Welded Joint of ∅336 mm x 31 mm Pipe of Martensite Heat Resistant Steel P91

    • Special Steel   Vol. 36, Issue 1, Pages: 60-61(2015)
    • Received:29 July 2014,

      Online First:31 August 2022,

      Published:31 August 2015

    移动端阅览

  • 赵振铎, 陈金虎, 原凌云, et al. Structure and Mechanical Properties of Welded Joint of ∅336 mm x 31 mm Pipe of Martensite Heat Resistant Steel P91[J]. Special Steel, 2015, 36(1): 60-61. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Quenching and Partitioning(Q & P)Process on Structure and Mechanical Properties of Steel 25Si2Ni3
Influence of Niobium Content on Structure and Mechanical Properties of Steel Cr8WMo2V2SiNb
Effect of Si Content on Structure and Mechanical Properties of Ultra Supercritical Steam Turbine Rotor Steel 30Cr2Ni4MoV
Effect of Solution Treatment on Structure and Mechanical Properties of Nickel Base Alloy 690
Effect of Quenching Cooling Rate on Structure and Mechanical Properties of Heat-Resistant Steel lCrl2Ni3Mo2VN

Related Author

解西强
高文涛
时捷
王存宇
张方
刘建华
马党参
张占普

Related Institution

昆明理工大学机电学院
钢铁研究总院结构材料研究所.
鞍山钢铁集团公司
钢铁研究总院
河冶科技股份有限公司
0