Effect of Temperature on Magnetic Performance of 33EH High Quality Sintered NdFeB Permanent Magnets
更新时间:2026-01-21
    • Effect of Temperature on Magnetic Performance of 33EH High Quality Sintered NdFeB Permanent Magnets

    • Special Steel   Vol. 36, Issue 1, Pages: 45-48(2015)
    • Received:05 August 2014,

      Online First:30 August 2022,

      Published:30 August 2015

    移动端阅览

  • 王凌燕, 于旭光, 张翼, et al. Effect of Temperature on Magnetic Performance of 33EH High Quality Sintered NdFeB Permanent Magnets[J]. Special Steel, 2015, 36(1): 45-48. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Vacuum Conditioning Heat Treatment on Structure and Magnetic Properties of High Temperature Annealing Oriented Silicon Steel 30Q140 Cold Rolled Sheet by Nitrogen Protection
Advance in Production Technology of Cold Rolled Grain-Oriented Electrical Steels
Effect of Rare Earth Element on Structure and Magnetic Performance of Cold Rolled Non-Oriented Electrical Steel Products
A Study on Production Process and Magnetic Properties of Conventional Grain-Oriented Silicon Steel
An Analysis of Influence of Measurement Factors on Magnetic Properties of Cold-Rolled Silicon Steel Sheet

Related Author

李莉
张静
杨玲
付勇军
张辉
康永林
王全礼
夏兆所

Related Institution

湖北理工学院材料科学与工程学院
昆明理工大学冶金与能源工程学院
黄石市产品质量监督检验所
鞍钢股份有限公司技术中心
北京科技大学新金属材料国家重点实验室
0