您当前的位置:
首页 >
文章列表页 >
Effect of Argon Shielding Atmosphere on Burning Loss of Titanium in Steel lCrl8Ni9Ti in Electro-Slag Remelting Process
更新时间:2026-01-21
    • Effect of Argon Shielding Atmosphere on Burning Loss of Titanium in Steel lCrl8Ni9Ti in Electro-Slag Remelting Process

    • Special Steel   Vol. 36, Issue 1, Pages: 38-40(2015)
    • Received:25 August 2014,

      Online First:30 August 2022,

      Published:30 August 2015

    移动端阅览

  • 邓鹏辉, 周立新, 潘明旭, et al. Effect of Argon Shielding Atmosphere on Burning Loss of Titanium in Steel lCrl8Ni9Ti in Electro-Slag Remelting Process[J]. Special Steel, 2015, 36(1): 38-40. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Argon Gas Shielded on Burning Loss of Electroslag Remelting Valve Steel NCF3015 Aluminum and Titanium
Effect of Slag Ingredient on Ti Burning Loss Rate and Ingot Surface Quality of High Temperature Alloy 0Cr15Ni25Ti2MoAlVB
Effect of Electromagnetic Stirring on Temperature Field of ESR Ingot
Control of Carbon and Sulfur Content in Electroslag Remelting Pure Iron
A Study on Evaporation of Fluorides in Slag during Electroslag Remelting Process

Related Author

贾景岩
丁磊
赵鸿燕
白海军
厉英
李宝宽
任学平
苗晓

Related Institution

2江苏申源集团有限公司
合智熔炼装备(上海)有限公司
太原钢铁(集团)公司技术中心
东北大学材料与冶金学院
北京科技大学材料科学与工程学院
0