Cold-Work Hardening and Wear-Corrosion Resistance of Silver-Containing High-Nitrogen Nickel-Free Antibacterial Stainless Steel HNSAg
更新时间:2026-01-21
    • Cold-Work Hardening and Wear-Corrosion Resistance of Silver-Containing High-Nitrogen Nickel-Free Antibacterial Stainless Steel HNSAg

    • Special Steel   Vol. 36, Issue 6, Pages: 59-62(2015)
    • Received:23 June 2015,

      Online First:16 August 2022,

      Published:16 August 2015

    移动端阅览

  • 袁军平, 王昶, 陈绍兴, et al. Cold-Work Hardening and Wear-Corrosion Resistance of Silver-Containing High-Nitrogen Nickel-Free Antibacterial Stainless Steel HNSAg[J]. Special Steel, 2015, 36(6): 59-62. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0