Experiment on Primary Recrystallization Annealing Process of 0.42 % Cu Hi-B Steel Manufactured by Simulated CSP Flowsheet
更新时间:2026-01-21
    • Experiment on Primary Recrystallization Annealing Process of 0.42 % Cu Hi-B Steel Manufactured by Simulated CSP Flowsheet

    • Special Steel   Vol. 37, Issue 2, Pages: 66-69(2016)
    • Received:09 November 2015,

      Online First:08 August 2022,

      Published:08 August 2016

    移动端阅览

  • 马力, 赵刚, 黄儒胜, et al. Experiment on Primary Recrystallization Annealing Process of 0.42 % Cu Hi-B Steel Manufactured by Simulated CSP Flowsheet[J]. Special Steel, 2016, 37(2): 66-69. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Structure and Texture of CSP Cold-Rolled Sheet of Low Carbon Steel DC03
Influence of Cold Reduction on Structure and Properties of DQ Level Deep-Drawing Strip Steel
A Study on Evolution of Recrystallization Structure and Textures in an IF Steel during Batch Annealing Process
Evolution of Structure and Texture in 3 % Si Steel during Hot and Cold Rolling Process based on CSP Technology
Effect of Rolling Process on Structure, Texture and Properties of X80 Pipeline Steel

Related Author

罗年高
余驰斌
张云祥
杨海林
成小军
伍康勉
程晓杰
刘雅政

Related Institution

武汉科技大学材料与冶金学院
湖南涟源钢铁集团公司
北京科技大学材料科学与工程学院
包头钢铁集团公司薄板厂
北京科技大学冶金与生态工程学院
0