Numerical Simulation and Application on Optimization of Flow Control Device in 38 t Expansion Tundish for Casting Slab
|更新时间:2026-01-21
|
Numerical Simulation and Application on Optimization of Flow Control Device in 38 t Expansion Tundish for Casting Slab
Special SteelVol. 37, Issue 3, Pages: 1-4(2016)
作者机构:
首钢技术研究院冶金过程研究所,北京,100043
作者简介:
基金信息:
DOI:
CLC:
Received:25 December 2015,
Online First:02 August 2022,
Published:02 August 2016
稿件说明:
移动端阅览
张利君, 刘金刚, 宁林新, et al. Numerical Simulation and Application on Optimization of Flow Control Device in 38 t Expansion Tundish for Casting Slab[J]. Special Steel, 2016, 37(3): 1-4.
DOI:
张利君, 刘金刚, 宁林新, et al. Numerical Simulation and Application on Optimization of Flow Control Device in 38 t Expansion Tundish for Casting Slab[J]. Special Steel, 2016, 37(3): 1-4.DOI:
Numerical Simulation and Application on Optimization of Flow Control Device in 38 t Expansion Tundish for Casting Slab
The optimization of flow control device in 38 t expansion tundish from original 29 t for casting 250 mm X 2 000 mm slab at steelworks has been carried out by numerical simulation. The effect of number and position of dam and weir on flow field and residual time distribution ( RTD) curves of liquid in tundish has been studied. With comprehensive consideration of tundish metallurgical effect and production cost
the optimum design for control flow devices- current regulator + dam + weir is proposed. With the optimum structure the volume fraction of plug flow region in tundish is up to 77. 1%
the volume fraction of dead region decreases to 4. 2%. With using this structure in situ the qualified ratio of non- metallic inclusions in pipeline steel produced in non-stable casting condition increases to 95% from original 88%
obviously to increase the metallurgical function of tundish.