Production Practice of Sulphur Free-Cutting Steel SAE1144 by 100t DC EAF-LF-VD-CC Flowsheet
更新时间:2026-01-21
    • Production Practice of Sulphur Free-Cutting Steel SAE1144 by 100t DC EAF-LF-VD-CC Flowsheet

    • Special Steel   Vol. 37, Issue 2, Pages: 39-40(2016)
    • Received:26 October 2015,

      Online First:08 August 2022,

      Published:08 August 2016

    移动端阅览

  • 黄周华, 阙宗华, 董军. Production Practice of Sulphur Free-Cutting Steel SAE1144 by 100t DC EAF-LF-VD-CC Flowsheet[J]. Special Steel, 2016, 37(2): 39-40. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Production   Practice of  150 mm×150 mm  Concasting Billet of Steel  ML08Al
Process Practice of Gear Steel 20CrMnTiH Production with 70 t LD-LF-CC Flow Sheet at Chengde Jianlong Steel
Process Practice of a 70 t High Impedance UHP Electric Arc Furnace
Practice of Process for Steelmaking of N80-1 Oil Casing Pipe Steel by 80 t Converter-LF-VD-CC Flow Sheet
Process Practice for Bearing Steel GCr15 Produced by 60 t BOF-LF (VD) -150 mm x 150 mm Casting Flow Sheet

Related Author

郑颖
郭平
石玉宏
张志宏
王海兵
苏雄杰
张勇
康建光

Related Institution

包头钢铁(集团)公司炼钢厂
承德建龙钢铁有限公司设计管理处
攀钢集团成都钢铁有限责任公司
东北大学材料与冶金学院
黑龙江建龙钢铁有限公司技术处
0