Calculation of Heat Transfer Coefficient of Heavy Rail Steel in Quenching Process Based on Finite Element Method
|更新时间:2026-01-21
|
Calculation of Heat Transfer Coefficient of Heavy Rail Steel in Quenching Process Based on Finite Element Method
Special SteelVol. 37, Issue 4, Pages: 13-17(2016)
作者机构:
内蒙古科技大学材料与冶金学院,包头,014010
作者简介:
基金信息:
DOI:
CLC:
Received:15 March 2016,
Online First:30 July 2022,
Published:30 July 2016
稿件说明:
移动端阅览
陈林, 王慧军, 陈昆宇, et al. Calculation of Heat Transfer Coefficient of Heavy Rail Steel in Quenching Process Based on Finite Element Method[J]. Special Steel, 2016, 37(4): 13-17.
DOI:
陈林, 王慧军, 陈昆宇, et al. Calculation of Heat Transfer Coefficient of Heavy Rail Steel in Quenching Process Based on Finite Element Method[J]. Special Steel, 2016, 37(4): 13-17.DOI:
Calculation of Heat Transfer Coefficient of Heavy Rail Steel in Quenching Process Based on Finite Element Method
A method to calculate the heat transfer coefficient is proposed by using finite element software combined with experimental calculation that is based on measured temperature curves
carrying out the nonlinear coupling on various factors which have influence on the heat transfer coefficient of U75V rail steel (/% : 0. 74C
0. 76Si
0. 82Mn
0. 014P
0. 028S
0. 071V)
the geometric model of the heat transfer coefficient of steel in quenching process is established and the heat transfer coefficient is obtained by iterative program of calculated heat transfer coefficient prepared with Python language. Using calculated heat transfer coefficient as a known boundary conditions
the simulation on temperature field of rail spray quenching coupled with phase transition in the DEFORM-3 D is carried out. The simulated-calculation cooling-curve corresponds to the measured cooling curve.