您当前的位置:
首页 >
文章列表页 >
Mathematical Modelling on Preventing Slag Entrapment of Liquid in Tundish during Tailing Slab Casting and Process Optimized Results
更新时间:2026-01-21
    • Mathematical Modelling on Preventing Slag Entrapment of Liquid in Tundish during Tailing Slab Casting and Process Optimized Results

    • Special Steel   Vol. 37, Issue 6, Pages: 17-21(2016)
    • Received:03 July 2016,

      Online First:26 July 2022,

      Published:26 July 2016

    移动端阅览

  • 王卫华, 刘洋, 赵新宇, et al. Mathematical Modelling on Preventing Slag Entrapment of Liquid in Tundish during Tailing Slab Casting and Process Optimized Results[J]. Special Steel, 2016, 37(6): 17-21. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Physical Simulation of Inclusion Removal and Slag Entrapment in 210 t RH Refining Process
A Study on Water Modeling of an 150 t Ladle Bottom Argon Blowing
Numerical Simulation of Effect of 100 t Bottom-Blowing Argon Ladle with Immersed Cylinder on Liquid Flow Field
Mathematic Simulation on Solidification Process of Φ210 mm Cast Round Bloom of Steel 37Mn5 for Petroleum Sleeve Tube and Process Optimization

Related Author

沈巧珍
吴墨环
彭明耀
肖尊湖
迟云广
吕明
刘福海
鲍翔

Related Institution

武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
华菱涟源钢铁有限公司
北京科技大学冶金与生态工程学院
辽宁科技大学材料与冶金学院
河北联合大学冶金与能源学院
0