Simulation and Optimization of Flow Control Device in 20t T-Type Tundish
更新时间:2026-01-21
    • Simulation and Optimization of Flow Control Device in 20t T-Type Tundish

    • Special Steel   Vol. 37, Issue 5, Pages: 1-4(2016)
    • Received:18 April 2016,

      Online First:27 July 2022,

      Published:27 July 2016

    移动端阅览

  • 彭家清, 白晓路, 贺银. Simulation and Optimization of Flow Control Device in 20t T-Type Tundish[J]. Special Steel, 2016, 37(5): 1-4. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Inner Structure of Tundish on Cleanliness of Casting Bloom
Numerical Simulation of Control Devices of Flow in a Two-Strand T-Shape 23 t Tundish and Structure Optimization
Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min

Related Author

唐海燕
李京社
包燕平
蒋静
李涛
吉传波
刘艳贺
贺铸

Related Institution

北京科技大学冶金与生态工程学院
武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
内蒙古科技大学材料与冶金学院
天津钢管集团技术中心
上海大学省部共建高品质特殊钢冶金与制备国家重点实验室
0