Effect of Non-Sine Oscillation of Mold on Lubrication of Mold Flux and Surface Quality of Cast Billet
更新时间:2026-01-21
    • Effect of Non-Sine Oscillation of Mold on Lubrication of Mold Flux and Surface Quality of Cast Billet

    • Special Steel   Vol. 38, Issue 3, Pages: 53-55(2017)
    • Received:15 December 2016,

      Online First:21 July 2022,

      Published:21 July 2017

    移动端阅览

  • 白晓路, 彭家清, 李孟雄. Effect of Non-Sine Oscillation of Mold on Lubrication of Mold Flux and Surface Quality of Cast Billet[J]. Special Steel, 2017, 38(3): 53-55. DOI:

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Process Optimization Steel 30CrMnSiA Production by EAF+LF(VD)-ESR  Combined  Process
Process Practice for Reducing Corner Transverse Crack of Cast Slab of Steel A36 Bearing B
Effect of Remelting Parameters Control with 70CaF2-30Al2O3 Slag Series on Surface Quality of Lower Part of ESR Ingot
Process Practice of Improvement on Surface Quality of 150 mm x 150 mm Casting Billet of Martensite Stainless Steel 2Cr13
Mathematic Simulation on Solidification Process of Φ210 mm Cast Round Bloom of Steel 37Mn5 for Petroleum Sleeve Tube and Process Optimization

Related Author

周从惠
张洲
于学森
彭其春
童志博
曹建新
刘红军
周春泉

Related Institution

大冶特殊钢股份有限公司
武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
湖南华菱涟源钢铁公司
湖北新冶钢有限公司炼钢事业部
北京科技大学钢铁冶金新技术国家重点实验室
0