Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6
|更新时间:2026-01-21
|
Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6
Special SteelVol. 38, Issue 1, Pages: 39-41(2017)
作者机构:
1. 抚顺特殊钢股份有限公司1技术中心
2. 技术处
3. 第三炼钢厂,抚顺,113001
作者简介:
基金信息:
DOI:
CLC:
Received:21 August 2016,
Online First:28 July 2022,
Published:28 July 2017
稿件说明:
移动端阅览
马群, 孙常亮, 冯桂萍, et al. Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6[J]. Special Steel, 2017, 38(1): 39-41.
DOI:
马群, 孙常亮, 冯桂萍, et al. Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6[J]. Special Steel, 2017, 38(1): 39-41.DOI:
Process Practice for Improvement of B-Type Inclusions in ESR Sulfur-Bearing Steel 34CrNiMo6
0.15~0.30Mo)的冶金流程为30 t EAF-LF-VD-浇铸Φ470 mm电极-3.6 t ESR锭(Φ610 mm)-锻成Φ280 mm棒材。在分析冶炼过程中影响钢中B类夹杂物级别因素的基础上
通过将电极氧含量从20×10
-6
降至11×10
-6
、同时电极S含量由0.035%提高到0.045%
进而减少重熔过程FeS等附加剂的添加量
将萤石-Al
2
O
3
-SiO
2
-MgO重熔渣系中萤石由45%提高到60%及SiO
2
由15%降低到5%等措施
生产钢材的B类夹杂物级别由原先的2.5级降至≤1.5级
并且钢中硫分布均匀适中
保证了电渣钢的质量。
Abstract
The metallurgical flowsheet of steel 34CrNiMo6 (/% : 0. 30 ~0. 38C
0.50 〜0. 80Mn
≤0. 40Si
0.015 ~0.035S
≤0.035P
1.30 〜1.70Ni
1. 30 〜1.70Cr
0. 15 ~0. 30Mo) is 30 t EAF-LF-VD-casting Φ70 mm electrode- 3. 6 t ESR ingot (Φ 610 mm)- forged to Φ280 mm round bar. Based on analysis the factors to influence rating of B-type inclusions in steel during steelmaking process
with using the measures including decreasing the oxygen content in electrode from original 20 x 10 to 11 x 10
-6
and increasing the S content in electrode from 0.035% to 0.045% to decrease the adding amount of FeS etc additives during ESR process
increasing the fluorite content in fluorite-Al
2
O
3
-SiO
2
-MgO ESR slag series from 45
% to 60% and decreasing the SiO
2
from 15% to 5%
the rating of B-type inclusions in round bar decreases from original 2. 5 to ≤ 1. 5 and the distribution of sulfur in steel uniform to insure the quality of ESR steel.