Optimization of Cooling Process of Extruding Needle in Hot Extrusion of Austenite Stainless Steel Tube
|更新时间:2026-01-21
|
Optimization of Cooling Process of Extruding Needle in Hot Extrusion of Austenite Stainless Steel Tube
Special SteelVol. 37, Issue 5, Pages: 32-35(2016)
作者机构:
1. 山西太钢不锈钢钢管有限公司,太原,030008
2. 武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室,武汉,430081
作者简介:
基金信息:
DOI:
CLC:
Received:20 April 2016,
Online First:29 July 2022,
Published:29 July 2016
稿件说明:
移动端阅览
王伯文, 刘升, 康喜唐, et al. Optimization of Cooling Process of Extruding Needle in Hot Extrusion of Austenite Stainless Steel Tube[J]. Special Steel, 2016, 37(5): 32-35.
DOI:
王伯文, 刘升, 康喜唐, et al. Optimization of Cooling Process of Extruding Needle in Hot Extrusion of Austenite Stainless Steel Tube[J]. Special Steel, 2016, 37(5): 32-35.DOI:
Optimization of Cooling Process of Extruding Needle in Hot Extrusion of Austenite Stainless Steel Tube
并计算得出生产不同规格钢管时挤压针的规格和所需水体积。Φ57.0 mm×6.3 mm~Φ139.7 mm×20.0 mm TP304不锈钢管的生产应用
结果表明
冷却工艺改进后
外径<100 mm挤压针的使用寿命由50~100次/支增加到100~150次/支
外径≥100 mm挤压针的使用寿命由100~200次/支提高到150~250次/支
显著降低成本和提高生产率。
Abstract
By finite element software Ansys the simulation on temperature and heat transfer of tool and die in hot extrusion process of TP304 austenite stainless steel tube to get the distribution of temperature and heat flux of die steel X38CrMoV5-3 extruding needle in hot extrusion process and the specification parameters and needed water volume for extruding different tube sizes are obtained by calculation. The application of production of φ57.0 mm X 6.3 mm~φ139.7 mm x 20.0 mm TP304 austenite stainless steel tubes show that with improvement o£ cooling process the service life of extruding needle with outside diameter <100 mm increases from 50~100 times/per piece to 100~150 times/per piece
and that with outside diameter ≥100 mm increases from 100~200 times/per piece to 150~200 times/per piece