Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min
|更新时间:2026-01-21
|
Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min
Special SteelVol. 37, Issue 5, Pages: 22-25(2016)
作者机构:
1. 内蒙古科技大学材料与冶金学院,包头,014010
2. 天津钢管集团技术中心,天津,300301
3. 上海大学省部共建高品质特殊钢冶金与制备国家重点实验室,上海,200072
作者简介:
基金信息:
DOI:
CLC:
Received:16 May 2016,
Online First:28 July 2022,
Published:28 July 2016
稿件说明:
移动端阅览
阮飞, 张红强, 刘智宇, et al. Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min[J]. Special Steel, 2016, 37(5): 22-25.
DOI:
阮飞, 张红强, 刘智宇, et al. Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min[J]. Special Steel, 2016, 37(5): 22-25.DOI:
Numerical Simulation of Influence of Flow Control Device on Transfer Performance in Tundish for H-Beam Bloom Casting with Speed 0.8 m/min
Based on tundish with length 8 m and liquid level 0.8 m for 3-strands H-beam bloom casting
the effect of curved dam flow-guiding hole diameter D(100~200 mm) and hole height H(350~550 mm) and angle between two flowguiding hole θ(20°~50°) on distribution of tundish liquid flow field and temperature field
liquid mixing status and removal of inclusions with different size has been simulated and studied by using three dimensional geometry model established with FLUENT soft ware. Results show that with flow-guiding hole diameter D 100 mm and height H 550 mm
and angle between two flow-guiding hole 0 50°
the comprehensive transfer performance in tundish is best