Effect of Channel Liquid Filter on Flow Field in Tundish for Two Strands Slab Continuous Casting
|更新时间:2026-01-21
|
Effect of Channel Liquid Filter on Flow Field in Tundish for Two Strands Slab Continuous Casting
Special SteelVol. 37, Issue 5, Pages: 17-21(2016)
作者机构:
1. 江西理工大学冶金与化学工程学院,赣州,341000
2. 钢铁研究总院国家连铸中心,北京,100081
作者简介:
基金信息:
DOI:
CLC:
Received:11 May 2016,
Online First:28 July 2022,
Published:28 July 2016
稿件说明:
移动端阅览
赵丹婷, 刘爱强, 仇圣桃, et al. Effect of Channel Liquid Filter on Flow Field in Tundish for Two Strands Slab Continuous Casting[J]. Special Steel, 2016, 37(5): 17-21.
DOI:
赵丹婷, 刘爱强, 仇圣桃, et al. Effect of Channel Liquid Filter on Flow Field in Tundish for Two Strands Slab Continuous Casting[J]. Special Steel, 2016, 37(5): 17-21.DOI:
Effect of Channel Liquid Filter on Flow Field in Tundish for Two Strands Slab Continuous Casting
Based on similarity principle and by established geometric similarity ratio 0.28:1 water model
the simulation test on flow field in 63.27 t tundish for two strands 230 mm x 1300 mm slab casting has been carried out to study the effect of channel filter on tundish liquid flow situation. Results show that only with turbulence inhibitor + wall and dam the plug flow area in tundish is relatively smaller and the dead area is rather larger; with placing dam by channel liquid filter the optimization effect is obvious and the installation is simplified with low cost
and the average resident time of liquid in optimized tundish increases from 348.22 s to 400.15 s
the peak time increases from original 172.4 s to 196.0 s and the dead volume decreases from 22.49% to 9.69%.