Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement
Smelting and Solidification | 更新时间:2025-05-09
    • Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement

    • Special Steel   Vol. 45, Issue 2, Pages: 61-65(2024)
    • DOI:10.20057/j.1003-8620.2023-00081    

      CLC: TF03+3
    • Received:22 May 2023

      Published:30 March 2024

    移动端阅览

  • Su Yongze,Zhang Xingli,Dai Fangyin,et al.Analysis of Surface Defects of High Strength Welding Wire Steel N2M2T Continuous Casting Billet and Process Improvement[J].Special Steel,2024,45(02):61-65. DOI: 10.20057/j.1003-8620.2023-00081.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Ingredient Design of 1Cr13 Stainless Steel Continuous Casting Protective Slag
Optimization Practice of 15CrMoG Rectangular Billet Protection Slag
Analysis on Corner Cracks of Angle Steel Q420C Rolled from 180 mm x 180 mm Cast Billet and Process Improvement

Related Author

Zhu Liguang
Song Lei
Wang Xinjuan
Qu Shuo
Yuan Zhipeng
Zhang Junwei
Hao Wenquan
Yan Hao

Related Institution

School of Metallurgy and Energy, North China University of Science and Technology
College of Materials and Engineering, Hebei University of Science and Technology
Hot Rolling Division, TangSteel Company, Hesteel Group
Technology Research Institute of Qingdao Special Iron & Steel Co., LTD.
钢铁研究总院冶金工艺研究所
0