Development of Extra-thick Plate 12Cr2Mo1VR(H) for Hydrogenation Reactor with 200 mm Thickness
Product Research and Development | 更新时间:2025-05-09
    • Development of Extra-thick Plate 12Cr2Mo1VR(H) for Hydrogenation Reactor with 200 mm Thickness

    • Special Steel   Vol. 45, Issue 2, Pages: 24-29(2024)
    • DOI:10.20057/j.1003-8620.2023-00163    

      CLC: TG142.1
    • Received:05 August 2023

      Published:30 March 2024

    移动端阅览

  • Yang Yang,Li Zhongbo,Bie Jiabao.Development of Extra-thick Plate 12Cr2Mo1VR(H) for Hydrogenation Reactor with 200 mm Thickness[J].Special Steel,2024,45(02):24-29. DOI: 10.20057/j.1003-8620.2023-00163.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

No data

Related Author

No data

Related Institution

No data
0