Wang Weimin,Qi Haiquan,Han Xiangnan,et al.Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel[J].Special Steel,2024,45(02):79-85.
Wang Weimin,Qi Haiquan,Han Xiangnan,et al.Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel[J].Special Steel,2024,45(02):79-85. DOI: 10.20057/j.1003-8620.2023-00164.
Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel
The influence of 82B steel with Mo (mass fraction) of 0.02%, 0.04%, 0.07% and 0.11% on microstructures and properties after high temperature stretching at different temperatures and the toughness mechanism of Mo element on 82B high carbon steel were studied. The results showed that:(1) During 200-300 ℃ high temperatures tensile, four groups of experimental steels had good mechanical properties , at 300 ℃ to reach the peak, it was optimal experiment group with Mo content 0.11% , tensile strength increased from 1 139 MPa to 1 192 MPa, yield strength slightly reduced to 736 MPa, elongation and section shrinkage significantly increased to 22% and 72.9%. Compared to the experimental steels with 0.02% Mo content, the yield strength reduced by about 5%, but the tensile strength increased by 5%, the elongation and section shrinkage increased significantly, and the plasticity increased simultaneously with the Mo content, with the temperature continued to rise, the mechanical properties tended to decrease as the materials start to soften.(2) When the Mo content was 0.02% and 0.04%, the microstructures except carburite gradually increased with the increasing of tensile temperature, sorbite and pearlite did not appear obvious changes, and the same as room temperature, when the Mo content increased to 0.07% and 0.11%, sorbite and pearlite clusters are progressively finer and more evenly distributed. At the same time, four groups of experimental steels showed blue brittleness during high temperature tensile at 300 ℃,through the fractures observation found that there was Al, Si and other elements of inclusions, and failure mode was ductile fracture, the fracture can mainly be divided into the shear lip areas and fiber areas,the shear lip areas with the increase in temperature gradually reduced.
Kant Thakur S , Harish L , Kumar Das A , et al . Hot deformation behavior and processing map of Nb-V-Ti micro-alloyed steel [J]. Materials Today: Proceedings , 2020 , 28 : 1973 - 1979 .
Chen Y , Zhang X M , Cai Z H , et al . Effect of microalloying with V and Ti on the microstructure and properties of electron beam welded thick high-Mn TWIP steel plates [J]. Materials Science and Engineering: A , 2021 , 811 : 141062 .
Wang C , Yu L M , Ding R , et al . Microstructure and mechanical properties of a novel medium Mn steel with Cr and Mo microalloying [J]. Materials Science and Engineering: A , 2021 , 825 : 141926 .
Moon J , Kim S D , Lee C H , et al . Strengthening mechanisms of solid solution and precipitation at elevated temperature in fire-resistant steels and the effects of Mo and Nb addition [J]. Journal of Materials Research and Technology , 2021 , 15 : 5095 - 5105 .
Wang B , Xiang S , Liang Y . Effect of microstructure on mechanical properties of high carbon steel wire rod [J]. Advanced Materials Research , 2013 , 842 : 31 - 34 .
Jo H H , Shin C , Moon J , et al . Mechanisms for improving tensile properties at elevated temperature in fire-resistant steel with Mo and Nb [J]. Materials & Design , 2020 , 194 : 108882 .
Janardhan G , Kishore K , Mukhopadhyay G , et al . Fatigue properties of resistance spot welded dissimilar interstitial-free and high strength micro-alloyed steel sheets [J]. Metals and Materials International , 2021 , 27 ( 9 ): 3432 - 3448 .
QUAN-LI W , FEI L , GONG-YAN Z , et al . Development of Cr, V Microalloyed SWRH82B Wire Rod Produced by CC-CR with 130 mm×130 mm Billet; proceedings of the 第五届国际低合金高强度钢会议暨第三届国际超细晶粒钢会议, 中国三亚, F, 2005 [C]: 581 - 586 .
Wan R C , Sun F , Zhang L T , et al . Effects of Mo on high-temperature strength of fire-resistant steel [J]. Materials & Design , 2012 , 35 : 335 - 341 .
Wan R C , Sun F , Zhang L T , et al . Development and study of high-strength low-Mo fire-resistant steel [J]. Materials & Design (1980-2015), 2012 , 36 : 227 - 232 .
Uemori R , Chijiiwa R , Tamehiro H , et al . AP-FIM study on the effect of Mo addition on microstructure in Ti-Nb steel [J]. Applied Surface Science , 1994 , 76-77 : 255 - 260 .
Chen L , Kim H S , Kim S K , et al . Localized deformation due to portevin–LeChatelier effect in 18Mn–0.6C TWIP austenitic steel [J]. ISIJ International , 2007 , 47 ( 12 ): 1804 - 1812 .
Gerstgrasser M , Smolenicki D , Akbari M , et al . Analysis of two parameter identification methods for original and modified Johnson-Cook fracture strains, including numerical comparison and validation of a new blue-brittle dependent fracture model for free-cutting steel 50SiB8 [J]. Theoretical and Applied Fracture Mechanics , 2021 , 112 : 102905 .
Koyama M , Shimomura Y , Chiba A Y , et al . Room-temperature blue brittleness of Fe-Mn-C austenitic steels [J]. Scripta Materialia , 2017 , 141 : 20 - 23 .
Yoshida S , Okumura T , Kita H , et al . High temperature tensile properties and its mechanism in low-carbon Nb-bearing steels [J]. Materials Transactions , 2014 , 55 ( 6 ): 899 - 906 .
Hutchinson B , Ridley N . On dislocation accumulation and work hardening in Hadfield steel [J]. Scripta Materialia , 2006 , 55 ( 4 ): 299 - 302 .