您当前的位置:
首页 >
文章列表页 >
Composition Design and Heat Treatment Welding Process Analysis of High‑manganese Austenitic Cryogenic Steel
Overview | 更新时间:2025-05-09
    • Composition Design and Heat Treatment Welding Process Analysis of High‑manganese Austenitic Cryogenic Steel

    • Special Steel   Vol. 45, Issue 2, Pages: 8-17(2024)
    • DOI:10.20057/j.1003-8620.2023-00227    

      CLC: TF642;TG161
    • Received:08 November 2023

      Published:30 March 2024

    移动端阅览

  • Xu Hao,Liu Jianhua,Liu Hongbo,et al.Composition Design and Heat Treatment Welding Process Analysis of High‑manganese Austenitic Cryogenic Steel[J].Special Steel,2024,45(02):8-17. DOI: 10.20057/j.1003-8620.2023-00227.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Heat Treatment Process on Microstructure and Properties of Forged 430F Ferritic Stainless Steel
Composition-Structure-Properties and Process Comprehensive Control Technology of 125ksi Super Martensitic Oil Well Pipe Material
Effect of Boron on the Microstructure and Strength-Toughness of Fe-Cr-B-C Alloy after Heat Treatment
Effects of LB/M Duplex Phase Heat Treatment on Microstructure and Mechanical Properties of Cold Working Die Steel DC53
Effect of Heat Treatment Temperature on Microstructure and Properties of 0Cr21Al6 Hot Rolled Sheet

Related Author

Guo Wei
Lu You
Zhang Xinge
Wang Wenquan
Ye Sainan
Xu Linchao
Du Liqing
Li Zaoyu

Related Institution

College of Optoelectronic Manufacturing, Zhe Jiang Industry & Trade Vocational College
School of Material Science and Engineering,Jilin University
Special Steel Institute of Central Iron and Steel Research Institute
Daye Specific Steel Co., Ltd.
Institute of materials & metallurgy, Inner Mongolia University of Science & Technology
0