Analysis on Formation Cause of Cold-Drawn Rod longitudinal Crack of Low-Carbon High-Sulphur Free-Cutting Steel and Process Improved Measures
|更新时间:2026-01-21
|
Analysis on Formation Cause of Cold-Drawn Rod longitudinal Crack of Low-Carbon High-Sulphur Free-Cutting Steel and Process Improved Measures
Special SteelVol. 37, Issue 2, Pages: 47-48(2016)
作者机构:
河南济源钢铁集团有限公司科技质量处,济源,459000
作者简介:
基金信息:
DOI:
CLC:
Received:03 November 2015,
Online First:08 August 2022,
Published:08 August 2016
稿件说明:
移动端阅览
万长杰, 白瑞娟, 申丽娟, et al. Analysis on Formation Cause of Cold-Drawn Rod longitudinal Crack of Low-Carbon High-Sulphur Free-Cutting Steel and Process Improved Measures[J]. Special Steel, 2016, 37(2): 47-48.
DOI:
万长杰, 白瑞娟, 申丽娟, et al. Analysis on Formation Cause of Cold-Drawn Rod longitudinal Crack of Low-Carbon High-Sulphur Free-Cutting Steel and Process Improved Measures[J]. Special Steel, 2016, 37(2): 47-48.DOI:
Analysis on Formation Cause of Cold-Drawn Rod longitudinal Crack of Low-Carbon High-Sulphur Free-Cutting Steel and Process Improved Measures
The crack phenomenon of cold-drawn Φ12 mm bar of low-carbon high-sulphur free cutting steel (/% : 0.07 C
1.24Mn
0.06P
0.39S) produced by 100t BOF-LF-165 mm x 165 mm casting billet -Φ14 mm hot-rolled bar-cold drawn to Φ12 mm rod process has been systematically analyzed to get the main cause of cold-drawn rod longitudinal crack is the billet inner defect formed in steelmaking and casting process by slag enclosure and oxidation etc factors. With the process measures including controlling mold cooling water rate in casting process
using weak secondary water cooling process with ratio water amount 0.83 L/kg
casting speed 1.5 m/min
non-oxidizing shielding casting and using viscosity 0.6 Pa·s at 1300℃ specialty mold powder
the occurrence of cold-drawn rod longitudinal crack is effectively avoided.