[1] |
Song Jingling, Zhou Xuan, Li Henghua.
Whole Process Cleanliness Analysis and Process Improvement of Petroleum Casing Steel 37Mn5
[J]. Special Steel, 2023, 44(4): 58-64.
|
[2] |
CHEN Xiujun, BI Sheng, ZHOU Weiji, YAO Yudong, WANG Xin.
Smelting Process Optimization Practice for Cold Heading Steel 10B21
[J]. Special Steel, 2022, 43(4): 63-65.
|
[3] |
Li Heyi, Wang Yi, Yang Hao, Ren Jianzhong, Wu Haoming.
Preventive Measures of Widmanstatten Structure of 0.45 % C Steel for Automobile Piston Rod and Process Optimization
[J]. Special Steel, 2021, 42(5): 69-71.
|
[4] |
Zhuo Weiwei, Zhang Bo, Liu Lang , Li Chunxiao.
Production Practice of Ti Microalloying and Rolled Products Cooling Process Optimization of Steel HRB400
[J]. Special Steel, 2018, 39(6): 22-24.
|
[5] |
Peng Jun, Wan Wuxia, Li Fuhua , Tang Ke.
Practice of Rolling Process for Φ 158.75 mm x25.4 mm Heavy Wall Tube of Martensite Stainless Steel 420M
[J]. Special Steel, 2018, 39(4): 35-37.
|
[6] |
Yang Yongjie, , Liu Yuai, Zhang Xiangyong.
Production Practice of Preventing Nozzle Clogging for Casting Ti-Bearing Welding Wire Steel GF50-G
[J]. Special Steel, 2018, 39(3): 9-12.
|
[7] |
Deng Birong, Zhang Bo, Zhou Jianfeng, Liu Lang , Li Chunxiao.
Effect of 210 t RH Refining Parameters on Cleanliness of Steelmaking-Rolling IF Steel and Process Optimization
[J]. Special Steel, 2018, 39(3): 31-34.
|
[8] |
Yu Xuesen , Zuo Longfei , Li Yang , Ma Han.
Process Practice for Improving Fatigue Life of Steel 60Si2MnA for Auto Stabilizing Rod
[J]. Special Steel, 2017, 38(2): 30-32.
|
[9] |
Zhang Liwu , Yao Na.
Practice of Process for Pronging Service Life of Tapping Hole of a 60 t BOF
[J]. Special Steel, 2017, 38(1): 36-38.
|
[10] |
Yang Yongchao , Wang Mingtao , Bai Jingang , Yang Yongjie.
Optimization of Annealing Process for 3 mm Hot-Rolled Strip Coil of Stainless Steel SUS410L
[J]. Special Steel, 2016, 37(2): 41-43.
|
[11] |
Chen Zhenye, Zhang Kuobin, Wang Yunge, Yin Shaojiang, Li Jianxin, Liu Tieli.
Analysis on Formation of Surface Longitudinal Crack of Steel Q235B and Q345B Medium-Heavy Plate and Process Optimization
[J]. Special Steel, 2015, 36(6): 30-32.
|
[12] |
Zhou Jianfeng , Luo Gang.
Optimization of 210 t RH Decarburization Process for Ultra-Low Carbon Steel Refining
[J]. Special Steel, 2015, 36(6): 33-35.
|
[13] |
Gao Ju , Ding Zhijun , Li Hui.
Analysis on Influence Factors of Control of Inclusions in Gear Steel 20CrMnTiH (TS) and Process Optimization
[J]. Special Steel, 2015, 36(5): 39-42.
|
[14] |
Li Xiaolong , Zhou Lixin , Zhou Dunshi , Feng Liang.
Finite Element Simulation on Wearing of Roll for Rough Mill of Hot Continuous Rolling Mill and Process Optimization
[J]. Special Steel, 2015, 36(2): 21-24.
|
[15] |
Yan Qingzhong , Chen Lie , Li Fawen , Zuo Hui , Wu Bin , Lu Yanming , Li Zheng , Zhao Haidong , Cheng Guoguang.
Optimization on Remelting Process of 1.1 t ESR Ingot of Blade Steel 1Cr12Ni2Mo2VN
[J]. Special Steel, 2015, 36(2): 44-47.
|