[1] |
Chen Hao, Sun Yibin, Xie Qingmin, Liu Xiaolong, Zhang Cunshuai, Peng Zhixian, Cheng Zhaoyang, Liu Jing.
Effect of Rare Earth Content on Microstructure and Corrosion Resistance of HRB400 Steel
[J]. Special Steel, 2025, 46(3): 58-65.
|
[2] |
Zhu Yincun, Song Changjiang, Tian Yuxin.
Influence Factors on σ-Phase Precipitation of FeCr16 Corrosion-resistant Soft Magnetic Alloy
[J]. Special Steel, 2025, 46(2): 62-66.
|
[3] |
Zhao Bo, Wang Shanbao, Xie Degang, Yuan Qin, Ai Fangfang, Wang Xixiang, Guo Jinmei.
Microstructure and Properties of Seamless Steel Pipe Gr.6 after Rolling and Normalizing
[J]. Special Steel, 2024, 45(6): 102-107.
|
[4] |
Li Yang, Chen Changyong, Fang Yong, Ma Shuai, Zhang Mina, Jiang Zhouhua.
Effect of Cu on the Mechanical and Corrosion Resistance of
Ferritic Stainless Steel Containing Sn
[J]. Special Steel, 2024, 45(3): 49-55.
|
[5] |
Tian Shuai, Zhang Xueling, Liu Zhenbao, Wang Xiaohui, Wang Changjun, Sun Yongqing, Yang Zhiyong, Qi Yue.
Effect of Niobium Alloying on the Corrosion Fatigue Properties of the Cr-Co-Ni-Mo Series of Ultra-high Strength Stainless Steels
[J]. Special Steel, 2024, 45(1): 103-110.
|
[6] |
Shi Yongxin , Li Qing , Zhong Qingyuan , Tian Wei , Ye Qiang.
Study on Homogenization Process of Super Austenitic Stainless Steel 254SMo
[J]. Special Steel, 2023, 44(2): 12-16.
|
[7] |
Zheng Jian , Peng Zhixian , Yuan Yuan , Huang Zhenhua , Yuan Zexi , Liu Jing.
Effect of Cu/Sb/Sn/Mo/W on Structure and Mechanical Properties of New National Standard 09CrCuSb Steel
[J]. Special Steel, 2023, 44(2): 84-89.
|
[8] |
Wu Zhuojie, Hou Lifeng, Du Huayun, Zou Yong, WuMin, Fan Guangwei, Wei Yinghui, .
Pitting Erosion Analysis of Ultra-Pure Ferritic Stainless Steel 445J2 and 316L Ultra-Low-Carbon Austenitic Stainless Steel in Lithium Bromide Solution
[J]. Special Steel, 2023, 44(1): 65-71.
|
[9] |
Li Xin , Wu Huajie , Liu Yinghui , Liu Wei.
Effect of Solid Solution Treatment on Corrosion Performance of As-cast 2101 Duplex Steel
[J]. Special Steel, 2022, 43(5): 86-91.
|
[10] |
Shi Yongxin, Li Qing, Zhong Qingyuan, Feng Wenjing, Chang Song , Wang Min.
Effect of Solution Temperature on Microstructure and Properties of Super Austenitic Stainless Steel 022Cr24Ni17Mo5Mn6NbN
[J]. Special Steel, 2022, 43(2): 82-84.
|
[11] |
Wang Baoshan, Zhang Hongliang, Liu Xin, Ma Jian , Feng Guanghong.
Strengthening Mechanism and Corrosion Resistance of 20MnSiV High Strength Steel Rebar Containing 0.23%Cr
[J]. Special Steel, 2022, 43(2): 85-89.
|
[12] |
Hou Yu, Geng Xin, Li Boyang, Li Xiaokai and Jiang Zhouhua.
Thermodynamic Analysis on Mineralogical Phase Precipitation in Cooling Process of Continuous Casting Mold Flux for Fe-Ni-Cr Alloy
[J]. Special Steel, 2022, 43(1): 1-5.
|
[13] |
Sun Ao, Liu Zhiwei, Zhang Ruiqi, Guo Xiaohong, Wu Chengju, Gao Hongtao, Sun Hang.
The Development and Properties study of High Weathering Structural Steels Q355GNH
[J]. Special Steel, 2022, 43(1): 53-56.
|
[14] |
Chen Zhenye, Qi Jianjun, Long Jie, Chen Zigang, Yang Hao , Lü Jianhui.
Development and Application of High Strength Corrosion Resistant and Wear Resistant Steel HNM450 in Complex Environment
[J]. Special Steel, 2021, 42(6): 50-54.
|
[15] |
Yan Daocong, Wang Zhenying, Ma Zhenyu, Zhu Xiaojie, ang Zhen.
Effect of Annealing Temperature on Microstructure and Properties of Ferrite Stainless Steel Y0Cr17SiS
[J]. Special Steel, 2021, 42(4): 78-80.
|