Abstract: The development of electric arc furnace (EAF) short process steelmaking is an important way for the iron and steel industry to realize the goal of "double carbon". In recent years, the modern EAF technology has been developing rapidly, and the bottom-blowing stirring technology of EAF is also progressing and being promoted, which makes an important contribution to the high efficiency and energy saving in production with EAF. This paper summarizes the mechanism, process characteristics, system composition, gas type, bottom blowing element type and process arrangement of the electric arc furnace, and summarizes the application of the bottom blowing technology. Simulation calculations shows that the flow rate of molten steel is obviously low in the area far away from the bottom blowing device. By arranging the bottom blowingdevice and optimizing the volume of bottom blowing gas in conjunction with the furnace characteristics, it is possible to effectively enhance the dynamic conditions of the molten pool, facilitate the mass transfer of elements within the molten steel, thereby achieving the goal of reducing energy and raw material consumption, and enhancing production efficiency.Therefore, it can be inferred that conducting research, combining different techniques such as blowing, power supply andpowder injection, formulating bottom blowing process system according to the characteristics of different new furnaces, as well as realizing intelligent bottom blowing are important directions for the development of short process steelmaking of modern EAF
Key words: EAF, Short Process Steelmaking, Bottom Blowing Stirring, Mathematical Simulation, Stirring Energy
摘要: 发展电弧炉短流程炼钢是钢铁工业实现“双碳”目标的重要途径。近年来,现代电弧炉技术发展迅速,电弧炉底吹搅拌技术也在不断进步和推广,对电弧炉生产的高效化和节能化作出了重要贡献。针对电弧炉底吹搅拌技术的机理、工艺特点、系统组成、气体种类、底吹元件类型及工艺布置方式进行综述,并对底吹技术的应用情况进行总结分析。模拟计算得出,远离底吹装置的区域,钢液流速明显偏低。结合炉型特点布置底吹装置及优化底吹气量,可改善熔池动力学条件,促进钢液元素传质,实现降低能耗和原材料消耗、提高生产效率的效果。深度开展底吹技术研发,与吹炼、供电、喷粉等工艺技术耦合,并结合新炉型特点制定底吹工艺制度,实现智能化底吹是发展现代电弧炉短流程技术的重要方向。
关键词: 电弧炉, 短流程炼钢, 底吹搅拌, 数值模拟, 搅拌能
CLC Number:
TF741. 5
He Qing, Yao Tonglu, Li Xiangchen, Zhao Jinxuan, Zhao Ge. Application and Deveopment of Bottom Blowing Stirring Technology to EAF[J]. Special Steel, 2024, 45(2): 1-7.
贺 庆, 姚同路, 李相臣, 赵进宣, 赵 舸. 底吹搅拌技术在电弧炉中的应用与发展[J]. 特殊钢, 2024, 45(2): 1-7.