Abstract: With regard to the forging cracking problem of 20 t flat ingot of N08120 nickel-based corrosion-resistant alloy, experiments and on-site process analysis were carried out. The solidification structure near the crack and crack surface composition were explored by macrostructure inspection, optical microscope and scanning electron microscope, combined with the equilibrium phase diagram and on-site data of the material , the comprehensive analysis showed that the cracking was caused by the internal solidification defects of the ingot and improper heating process before forging. During the solidification process, it was prone to form porosity and shrinkage defects in the lower middle part of the flat ingot, and there was a stacked charging mode of cold ingots during heating, resulting large tensile stress inside the ingot. When the stress value was higher than the internal bonding strength, cracks would initiate and expand outward during forging process. By reducing the casting speed of shrink head to 30% of that of ingot body, adding the heating agent in advance when the molten steel level reached 2/3 of height of the shrink head, increasing heating agent from 2 kg/t to 2.5 kg/t and adding carbonized rice husk in order to improve the insulation effect, increasing the proportion of hot-feeding ingots in the forging process and strictly prohibiting the stacking of cold ingots into the furnace, the problem of forging cracking was solved.
Key words: N08120 Nickel-based Alloy, Flat Ingot, Solidification Defect, Forging Cracking
摘要: 针对N08120镍基耐蚀合金20 t扁锭锻造开裂问题,开展了实验和现场工艺分析,利用低倍实验、光学显微镜和扫描电子显微镜等对裂纹附近的凝固组织和裂纹表面成分进行探究,并结合材料的平衡态相图和现场数据,综合分析可得,开裂是钢锭内部凝固缺陷和不恰当的锻造加热工艺共同导致的,在凝固过程容易在扁锭的中下部形成疏松、缩孔缺陷,且锻造加热时存在冷锭叠装的装炉方式,钢锭内部存在较大的拉应力,当应力值高于其结合强度的时候便会萌生裂纹,并在锻造过程向外扩展。通过降低帽口补注流速为锭身的30%,当补注至帽口2/3时提前加入发热剂,发热剂用量从2 kg/t提升至2.5 kg/t,并按照0.8 kg/t添加碳化稻壳保温,在锻造工序,提升热送钢锭比例,对于冷锭严禁叠装入炉,锻造开裂问题得以解决。
关键词: N08120镍基合金, 扁锭, 凝固缺陷, 锻造开裂
CLC Number:
TG316.2
Liu Yu, Xu Wenliang. Cause Analysis and Process Improvement Measures of Primary Forging Cracking for 20 t Flat Ingot of N08120 Nickel-based Corrosion-resistant Alloy[J]. Special Steel, 2025, 46(1): 39-43.
刘煜, 徐文亮. N08120镍基耐蚀合金20 t扁锭初锻开裂原因分析和工艺改进[J]. 特殊钢, 2025, 46(1): 39-43.