Abstract: The USTB(University of Science and Technology Beijing)furnace wall oxygen injection technology have been used for a 50 t EBT arc furnace and a 60 t shaft arc furnace at Nol melting shop at Fushun Steel by cooperation of Fushun Steel and University of Science and Technology Beijing. The application results showed that the tap to tap time re- duced by 4.9~7.2 min with 100% scrap charging and reduced by 9.4~10.9 min with 70% scrap and 30% hot metal charging; the electric power consumption decreased by 17.9~37.2 kWh/t,while oxygen consumption increased by ~4.5 m³/t.The service life of USTB oxygen lance was up to more than 1000 heats to get good economic and technical effect.
Key words: EAF Steelmaking, USTB Oxygen Injection, Hot Metal Charging
摘要: 抚顺特钢与北京科技大学合作在第一炼钢厂1座 50 t EBT电弧炉和 1座 60 t竖式电弧炉上采用USTB(北京科技大学 )炉壁氧气喷吹工艺。使用结果表明 ,全废钢炉料冶炼周期缩短4.9~7.2 min ,废钢 +30 %铁水冶炼周期缩短 9.4~10.9 min ,电耗降低17.9~37.2 kWh/t,氧耗增加~4.5m3/t。USTB氧枪的使用寿命达1000炉以上 ,取得了良好的经济技术效果
关键词: 电弧炉炼钢, USTB氧气喷吹, 铁水热装
Sun Liguo , Yan Lifeng , Li Shu , Xiao Lingzhi , Zhu Rong , Jiao Bing , Li Xiaoqiang , Wan Zhenzhou. Application of USTB Furnace Wall Oxygen Injection Technology for EAF Steelmaking at Fushun Special Steel[J]. Special Steel, 2005, 26(2): 41-42.
孙立国, 阎丽峰, 李 澍, 肖令之, 朱 荣, 焦 兵, 李晓强, 王振宙. 抚顺特钢电弧炉 USTB 炉壁氧气喷吹工艺的应用[J]. 特殊钢, 2005, 26(2): 41-42.
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2005/V26/I2/41