A Study on Simulation of Stirring and Scouring Action in Top and Bottom Combined Blown Converter at Chongqing Steel

Chen Dengfu1 , Wen Liangying1 , Dong Lingyan1 , Zhang Shengfu1 , Sun Yijie2 , Zhou Yuanhua2 , Yang Honglian2 , Li Bin2   

  1. 1. School of Materials Science and Engineering, Chongqing University, Chongqing 400044 ;
    2. Chongqing Iron and Steel Co Ltd, Chongqing 400084 ;
  • Received:2004-11-08 Online:2005-04-01 Published:2023-04-24
  • Contact: Wen Liangying

重钢复吹转炉熔池内的搅拌和冲刷作用的模拟研究

陈登福1,温良英1,董凌燕1, 张生富1,孙毅杰2,周远华2,杨洪莲2,李斌2   

  1. 1、重庆大学材料科学与工程学院,重庆 400044;
    2、重庆钢铁股份有限公司,重庆 400084;
  • 通讯作者: 温良英
  • 作者简介:陈登福,男,41岁,博士,教授。从事冶金研究和教学工作。

Abstract: According to characteristics of the depth of metal and slag, the furnace structure and size, and the revamping design for an top-blown converter (charging metal 85 t) modified to a top and bottom combined blown converter, a cold simulation model for top and bottom combined converter has been designed and established to test and study the effect of flow impinging on converter bath, the mixing characteristics of bath in different melting period and the scouring action of melt on furnace wall, the test results showed that the reasonable bottom blown strength was 0.06~0.11 m3/min▪t for the converter at Chongqing Steel; and in top and bottom blown, the bath mixing time was lowest by operation at basic lance location.

Key words: Converter, Top and Bottom Combined Blown, Cold Simulation Model, Bottom Blown Oxygen Strength, Scouring Action

摘要: 针对重钢顶吹转炉 (铁水装入量 85t)改造成顶底复吹转炉钢液和渣液深度及炉子结构、尺寸和改造设计的特点 ,设计制作了复吹转炉冷态模拟模型 ,实验研究了流股对熔池冲击作用效果 ,转炉不同炉役期熔池的搅拌混匀特性 ,熔体对炉壁的冲刷作用。实验结果得出重钢转炉在整个役期内合理的底吹供气强度为0.06~0.11 m3/min·t;顶底复吹时 ,基本枪位下操作对熔池搅拌混匀时间最短

关键词: 转炉, 复吹, 冷态模型, 底吹供气强度, 冲刷