ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (3): 41-44.

Previous Articles     Next Articles

Selection and Application of Cold Rolling Mill for Stainless Steel

Wang Yide   

  1. Taiyuan Iron and Steel(Group) Co Lid, Taiyuan 030003
  • Received:2004-12-09 Online:2005-06-01 Published:2023-05-26

不锈钢冷轧机的选择及应用

王一德   

  1. 太原钢铁(集团)有限公司,太原030003
  • 作者简介:王一德(1938-),男,教授级高级工程师。研究生毕业于 北京科技大学压力加工系,现从事不锈钢、电工钢的技术 改造工作。

Abstract: Secondary refining, continuous casting and multi-roll mill technology are three main and important technol- ogies to promote rapid development of stainless steel production in world. Aiming at deformation characteristics of the stain- less steel and basic requirements to the cold rolling mill, the commonly used single stand and reversing cold mill and cold tandem mill in recent plat and strip production for stainless steel - Sendzimir ZR mill, SUNDWIG four post mill and SMS- SB twin stand mill are introduced and described, of which the recent development is presented in this article.

Key words: Stainless Steel, Cold Rolling Mill, Sclection

摘要: 二次精炼、连铸和多辊轧机是促进世界不锈钢生产快速发展的三大重要技术。针对不锈钢变形 特点和对冷轧机的基本要求,重点介绍了当前不锈钢板带生产中普遍选用的森吉米尔 ZR轧机,SUNDWIG 四 立柱轧机和 SMS-SB双机架轧机等几种单机架可逆式冷轧机和冷连轧机,并对它们的近代发展作了描述。