ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (3): 57-58.

Previous Articles     Next Articles

Process Practice of Hot Forging Microalloying Steel F40MnV by Converter

Dai Guanwen, Liang Mei,Wu Yunfeng,Liu Xianming, Mao Tianrong,Chen Siliar,Wang Xinhu   

  1. Shijiashuang Iron and Steel Co Lid, Shijiashuang 050031
    Central Iron and Steel Research Institute, Beijing 100081
    University of Science and Technology, Beijing 100083
  • Received:2004-12-24 Online:2005-06-01 Published:2023-05-29

转炉生产热锻非调质钢 F40MnV 的工艺实践

戴观文 ,梁 玫,武云峰, 刘宪民,毛天荣,陈思联, 王新华   

  1. 石家庄钢铁有限责任公司,石家庄050031
    钢铁研究总院,北京100081
    北京科技大学,北京100083
  • 作者简介:戴观文,男,31岁,北京科技大学硕士研究生。研究方 向:高品质非调质钢的研究与开发。

Abstract: The φ25 mm bar of microalloying stocl F40MnV- 0.39~0.43C,1.20- 1.36Mn,0.07~0. 10V 0.009~0.024P,0.011~0.018S was produced by a 55 t converter + 60 t ladle refining fumace,150 mm×150 mm 4 strand concaster, short- stressed continuous rolling mill strain process. Okygen content in steel [0] was(18,8~20.5)x 10-6 and[N] was(35.2~53.2)×10-6,The chemical compositions, mechanical properties, cleanliness and micro- ant macrostructure of steel are all up to the requirement of standard and the demand of customers, VN alloy shall be selecter adding during microalloying of steel to increase the nitrogen content

Key words: Microalloying Steel F40MnV, Converter,Ladle Refining Fumacs

摘要: 采用55t 转炉+60t 钢包精炼炉,150mm×150mm4 流弧形连铸机,短应力连轧机组生产425 mm 非调质钢 F40MnV(%:0.39~0.43C,1.20-1.36Mn,0.07~0.10V,0.009~0.024P,0.011~0.018S)。钢中氧 含量[0]为(18.8-20.5)×10-6,[N]为(35.2~53.2)×10-6。钢的化学成分、力学性能、纯洁度、高低倍组织均 达到标准和用户要求。为控制钢中N 含量可选择加 VN 合金,在微合金化时增氮。

关键词: 非调质钢 F40MnV, 转炉, 钢包精炼炉