ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (3): 61-62.

Previous Articles    

Quality Control of Steel Blank for Tube of High Pressure Boiler by Concasting and Tandem Rolling at Xingcheng Special Steel

Ce Longgui, Li Guozhong   

  1. Jiangyin Xingcheng Special Steel Co Ltd, Jiangyin 214429
  • Received:2005-01-20 Online:2005-06-01 Published:2023-05-30

兴澄特钢连铸连轧高压锅炉管用钢坯的质量控制

葛龙桂, 李国忠   

  1. 江阴兴澄特种钢铁有限公司,江阴214429
  • 作者简介:葛龙桂(1969-),男,1992年毕业于北京科技大学压力加 工专业。从事轧钢工艺、电站锅炉高压用无缝钢管钢种的研究和开发。

Abstract: By using 100 t arc fumace steelmaking with hot metal + pig iron + quality sorap charging, LF secondary refining, concasting billet hot feeding(temperature for heat fumace ≥550 ℃),and automatic determinant system for quali- ty of concasting billet, the S, P content in steel tube blank for high pressure boiler including 20G,25MnG,SA-210C, 15CrMnG,12Cr1MoVG, SA-213 T12 designations produced at Xingcheng Special Steel was ≤0.025%,residual Cu≤ 0. 18%,(As+Sn+Sb+Pb+Bi)≤0.028%,and has higher cleanliness and quality  level  of products.

Key words: Tube Blank, Steel for Tube of High Pressure Boiler, Residual Deleterious Elements

摘要: 通过采用100t 电弧炉热装铁水+生铁+优质废钢冶炼、LF二次精炼,连铸坯热装(≥550℃), 连铸坯质量自动判定系统,兴澄特钢生产的20G,25MnG,SA-210C,15CrMoC,12Cr1MoVG,SA-213 TI2 等牌号的 高压锅炉管坯钢S、P含量≤0.025%,残余Cu≤0.18%,(As+Sn+Sb+Pb+Bi)≤0.028%, 并具有高的洁净度 和实物质量水平。