Development of a Measuring Device for Melting and Crystallization Parameters of Slag by Single Thermal Couple Method

Shi Jinliang, Jia Bi , Wu Yunjun, He Fenglei,  Li Jiaqing , Wen Guanghua , Tang Ping   

  1. 1. Chongqing Science and Technology College ‚Chongqing 4050 2. Chongqing University ‚Chongqing 404
  • Received:2005-04-01 Online:2005-08-01 Published:2023-04-17

热丝法炉渣熔化和结晶过程测定装置的研制

施金良,   贾  碧 , 吴云君,  贺丰雷,   李家庆 , 文光华,   唐  萍   

  1. 1.重庆科技学院 ,重庆 4050
    2.重庆大学 ,重庆 404
  • 作者简介:施金良(1963-) 男 高级工程师 1992年北京科技大学工业自动化硕士毕业。重庆科技学院电子信息工程学院副院长 ‚从事控制理论与控制工程、冶金检测设备研究

Abstract: A measuring device for melting and crystallization parameters of slag has been developed using single thermal couple which not only is as a measuring temperature element ‚but also as a heating element with the characteristics of ℃ for crystallizing temperature also was ±10℃ and the error for crystallizing rate of slag was ±5%.

摘要: 研制了热丝法炉渣熔化和结晶参数测定仪,该测定仪用一根双铂铑热电偶丝既作加热元件又作测温元件,具有升、降温速度快,测量效率高的特点。对板坯保护渣测试结果表明,炉渣开始熔化温度和流动温度的测量误差±10℃,结晶温度±10℃,结晶比率±5%。

关键词: 热丝法, 炉渣, 熔化温度, , 结晶温度, , 结晶率