Electroslag Remelting Casting of Steel 42CrMoA for Crankshafts of Diesel Engine

Zhang Zhenguo , Tang Feng   

  1. Dept of material and Chemical Engineering,Zhongyuan Technology College,Zhengzhou 450007
  • Received:2005-04-06 Online:2005-10-01 Published:2023-04-04

42CrMoA钢内燃机曲轴的电渣熔铸

张振国,汤 峰   

  1. 中原工学院材料与化学工程系,郑州 450007
  • 作者简介:张振国(1969-),男,讲师,1997年大连铁道学院毕业,从事材料教学和研究。

Abstract: The weight of one crankshaft finished product of steel 42CrMoA (0.34~0.49C,0.9~1.2Cr,0.15~ 0.25Mo) for diesel engine is about 1 t, for which the weight of forging blank is 6.2 t, while the weight of electroslag remelting(ESR)casting - welding blank in only 1.5 t.The chemical composition of steel 42CrMoA ESR casting blank is uniform, of which the cleanliness is high than that of forging blank. The results in service at 8240 diesel engine showed that as compared with forging crankshafts, there was no wear abrasion scaling observed to better resolve the problem about wear abrasion scaling off.

Key words: ESR Casting-Welding, Crankshaft of Diesel Engine, Steel 42CrMoA

摘要: 42CrMoA钢(%:0.34~0.49C,0.9~1.2Cr,0.15~0.25Mo)内燃机曲轴成品约重1t,用锻造生产其毛坯重6.2t,采用电渣熔铸-电渣熔焊法生产的坯重仅为1.5t。42CrMoA钢电渣熔铸件化学成分均匀,纯净度较锻件高。在8240柴油机上装车使用结果表明,与锻钢曲轴相比,没有观察到表面磨损脱落,较好地解决了曲轴的磨损脱落问题。