Structure and Properties of Low Carbon Sheet produced by FTSR Concasting Thin Slab Continuous Rolling Process at Tangshan Iron and Steel

Feng Yunli1 , Wang Linge2 , Chen Huahui1   

  1. 1. Material Science and Engineering,China University of Mining and Technology,Beijing 100083;
    2. Hebei Polytechnic University,Tangshan 063009;
  • Received:2005-03-09 Online:2005-10-01 Published:2023-04-04

唐钢FTSR连铸薄板坯热连轧低碳钢板的组织和性能

冯运莉1,王岭娥2,陈华辉1   

  1. 1. 中国矿业大学(北京校区)材料科学与工程系,北京 100083;
    2. 河北理工大学,唐山 063009;
  • 作者简介:冯运莉(1965-),女,副教授,在读博士,河北工业大学毕业,从事钢的组织性能研究和新产品开发。工作单位:河 北理工大学冶金与能源学院,唐山063009。

Abstract: The structure and properties of 3.5 mm strip of steel SS330 (0.04%~0.07%C) produced by FTSR(Flexible Thin Slab Rolling)process from 70 mm thin slab at Tangshan Iron and Steel.The results showed that the structure of FTSR hot rolled SS330 steel strip was uniform,the average grain size was 6.2~7.0 μm,yield strength 284~293 MPa,tensile strength 369~375 MPa,elongation 38%~42%

Key words: FTSR Process, Thin Slab, SS330 Low Carbon Steel, Structure, Mechanical Propertics

摘要: 试验了唐钢FTSR(FlexibleThinSlabRolling)薄板坯连铸连轧生产线从70mm薄板坯生产3.5mm SS330低碳钢带(0.04%~0.07%C)的组织和性能。结果表明,FTSR热轧3.5mm板带SS330钢组织均匀,平均晶粒尺寸为6.2~7.0μm,其屈服强度为284~293MPa,抗拉强度369~375MPa,延伸率38%~42%。

关键词: FTSR工艺, 薄板坯, SS330低碳钢, 组织, 力学性能