An Analysis on Surface Cracks Formation of H Beam of Nb-V Microalloying Steel BS55C

Liu Jianhua1,Bao  Yanping',Zhou  Jie1,Du  Songlin2,Li Jianzhong2, Tang  Yinbo2   

  1. 1 School of Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 Maanshan Iron and Steel Co Ltd,Maanshan 243002
  • Received:2005-07-15 Online:2006-02-01 Published:2006-02-01
  • Supported by:
    本课题为国家技术创新项目([2002]566)

Nb-V微合金化H型钢BS55C表面裂纹成因分析

刘建华1, 包燕平1, 周  杰1, 杜 松 林2, 李建中2, 汤寅波2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;2马鞍山钢铁股份有限公司,马鞍山243002
  • 作者简介:刘建华(1966-),男,博士,副教授,从事精炼连铸研究

Abstract: The causes of surface cracks formation of H beam of Nb-V microalloying steel BS55C-0. 14~0. 17C,0.45~0.55Si,1.25~1.45Mn,0.08~0. 10V,0.03~0.05Nb have been analyzed. The results showed that the steel was sensitive to longitudinal crack at solidification and its plasticity at 700~950 ℃ was lower,therefore,the cracks were easily produced at surface of H beam. Based on analysis of 168 heats production data of Nb-V microalloying steel BS55C,it was obtained that it was available to effectively decrease the surface cracks of H beam of Nb-V microalloying steel by using LF refining,controlling [s]≤0.015% and [P]≤0.020%,optimizing cast nozzle, adopting weak secondary water cooling and avoiding straightening at 700~900 ℃

摘要: 分析了成分为(%):0.14~0.17C,0.45~0.55Si,1.25~1.45Mn,0.08~0. 10V,0.03~0.05Nb H 型 钢BS55C表面裂纹形成原因。结果表明,该钢凝固时纵裂的敏感性较大,700~950℃范围内的塑性较低,使H 型钢表面易产生裂纹。由168炉Nb-V微合金化H 型钢BS55C生产数据分析得出,采用LF精炼,控制钢中S≤ 0.015%、P≤0.020%,优化浇铸水口,采用弱二次水冷工艺,避免在700~900℃范围矫直,可有效减少Nb-V微 合金化H 型钢的表面裂纹