Effect of 90 t LF(VD)Refining Process on Oxygen Content in Bearing Steel GCr15

Pang Hongliang, Bian Yanjun   

  1. Beiman Special Steel Beixing Co, Qiqihaer 161041
  • Received:2005-09-01 Online:2006-02-01 Published:2006-02-01

90tLF(VD)精炼工艺对 GCr15 轴承钢氧含量的影响

庞洪亮, 边延君   

  1. 北满特钢北兴公司,齐齐哈尔161041
  • 作者简介:庞洪亮(1973-),男,工程师,技术科科长。1995年佳木斯 工学院毕业,从事冶炼、轧钢质量攻关及生产工作

Abstract: The CCr15 bearing steel is produced by a 90 t EBT arc furnace-LF(VD)-240 mm×240 mm billet concasting process at Beiman Special Steel. The statistic results showed that with using 4.46 high basicity slag series,deoxidant containing 32.8% Al,VD vacuum treatment for 25 min and controlling [Als]≤0.030%,the oxygen content in GCr15 bearing steel was ≤8×10-6

摘要: 北满特钢用90tEBT 电弧炉-LF(VD)-240mm×240mm方坯连铸生产CCr15轴承钢。GCr15轴承 钢钢包精炼时采用碱度为4.46的高碱度渣系,用含32.8%Al的脱氧剂,并进行25 min VD真空处理,保持 [Als]≤0.030%,统计结果表明GCr15轴承钢的氧含量≤8×10-⁶