Development and Application of Magnesia Carbon Taphole Brick for a 60 t Utra-High Power Electric arc Furnace

Bo Yongming   

  1. Fushun Special Steel Co Ltd,Northeastemn Steel Group,Fushun 113001
  • Received:2005-09-08 Online:2006-02-01 Published:2006-02-01

60 t超高功率电弧炉用镁碳出钢口砖的研制与应用

薄永明   

  1. 东北特钢集团抚钢股份有限公司,抚顺113001
  • 作者简介:薄永明(1971-),男,工程师,1996年鞍山钢铁学院毕业, 从事耐火材料的应用技术工作及冶炼工艺的管理

Abstract: With basic material -85% first grade magnesia + 15% graphite, adding % Al/Mg(60/40)antioxidant, using solid and liquid phenolic resin as binder and making up according to reasonable grain grading, the magnesia-carbon taphole brick for two sets of 60 t ulra-high power electric arc furnace(UHP EAF)at Fushun Special Steel has been developed and was in service.The service life of taphole of developed brick increased to about 150 heats from original about 110 heats

摘要: 采用一级电熔镁砂85%、石墨15%的镁碳材料,加入3%Al/Mg(60/40)抗氧化剂,以固体、液体酚醛树脂为复合结合剂,按合理颗粒级配比所研制的镁碳出钢口砖用于抚钢2座60t超高功率电弧炉出钢口, 使出钢口使用寿命由约110炉次提高到约150炉次,满足了使用要求