[1] |
Liu Fubin, Jiang Zhouhua, Li Huabing, Feng Hao, Dong Junwei, Zhang Quyi, Zheng Huaibei.
Development of Pressurized Electroslag Remelting Equipment and Process Technology
[J]. Special Steel, 2024, 45(4): 26-33.
|
[2] |
Ni Bing, Cui Zhifeng, Shangguan Fangqin, Li Xiuping, Li Tao.
Overview on Carbon Reduction Routes of Three Types of Iron and Steel Manufacturing Processes
[J]. Special Steel, 2023, 44(5): 2-8.
|
[3] |
Lei Yinghua , Zhou Xu , Xiao Youyi , Zhang Yongqiang , Zhang Yi.
New Development of Research on Die Steel for Die-Casting Steel in China
[J]. Special Steel, 2022, 43(5): 1-6.
|
[4] |
Li Xiaolong Shi Tao, Chen Zhangming, Zhou Dunshi, Zhou Lixin.
Optimization Practice of Rolling Process for High-Strength Low-Alloy Steel Q420N
[J]. Special Steel, 2022, 43(1): 50-52.
|
[5] |
Han Changhai, Wang Zhili , Shi Jinqing.
Research and Development of Non-Quenched-Tempered Steel C70S6BY for Expanding Fracture Connecting Rod
[J]. Special Steel, 2021, 42(6): 55-57.
|
[6] |
.
Development and Practice of Low Alloy High Strength 30CrMnTi Steel Wire Rod
[J]. Special Steel, 2021, 42(1): 29-31.
|
[7] |
Chen Xingyu , Xu Zhen , Wang Ning , Zhang Yushun , Wang Hongjiang , Ding Taixing , Gao Yu.
Research Progress of High Strength Marine Engineering Steel Having Low Yield Ratio
[J]. Special Steel, 2020, 41(6): 1-5.
|
[8] |
Yin Weijiang , Li Jie, Long Jie, Zhang Jian, Yuan Jincheng, Wu Yanyang , Wang Tiantian.
Development and Application of 200 mm Extra Thick 12Cr2MolR Steel Plate for Hydrogen Chemical Industry
[J]. Special Steel, 2020, 41(3): 51-54.
|
[9] |
Cao Shuwei, Gao Xinjun , Sun Tuo.
Analysis on Forming Mechanism of Fine Cracks at Narrow Faces of Slab of HSLA Steel and Process Improvement
[J]. Special Steel, 2019, 40(5): 46-49.
|
[10] |
Yin Sheng, Zhu Hongdan.
Development of Yield Strength 750 MPa HSLA Steel for Container
[J]. Special Steel, 2019, 40(1): 16-18.
|
[11] |
Meng Chuanfeng, Wang Yide, Wei Yinghui, Cui Tianxie , Wang Yutian.
The Development of Mechanical Engineering of TQ960E Microalloyed High Strength Low Carbon Steel
[J]. Special Steel, 2018, 39(6): 66-70.
|
[12] |
Liu Nianfu.
Development of Gear Steel 20CrMnTiH with Narrow Hardenability Band
[J]. Special Steel, 2018, 39(1): 41-43.
|
[13] |
Wan Changjie , Shen Lijuan , Liu Mei , Zhao Tianli.
Development of High Carbon Microalloying Non-Quenched-Tempered Steel C70S6 and Process Practice
[J]. Special Steel, 2017, 38(5): 31-33.
|
[14] |
Chen Zhenye , Sun Li , Wang Xiaoshu , Wei Ming , Zhang Haijun.
Development of Low Yield Point Steel LY225 for Anti-Seismic Building
[J]. Special Steel, 2017, 38(2): 37-39.
|
[15] |
Deng Tongwu , Ke Xiaotao , Hu Fengrong.
Development of Non-Quenched-Tempered Vanadium Steel 48MnV for Pre-Hardening Plastic Die