ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2006, Vol. 27 ›› Issue (2): 40-42.

Previous Articles     Next Articles

Water Model Simulation Test for VOD Refining Process

Wang Dong1 , Bao Yanping1 , Xu Baomei1 , Li Jianmin2 , Li Zhibin2 , Li  Daoming2   

  1. 1. School of Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2. Taiyuan Iron and Steel(Group)Co.,Ltd., Taiyuan 030003;
  • Received:2005-11-04 Online:2006-04-01 Published:2023-03-02

VOD精炼过程的水模型实验

王 东1,包燕平1,徐保美1,李建民2,李志斌2,李道明2   

  1. 1. 北京科技大学冶金与生态工程学院,北京 100083;
    2. 太原钢铁(集团)有限公司,太原030003;
  • 作者简介:王东(1978-),男,硕士研究生,从事钢包、中间包及结晶器的水模拟研究。

Abstract: The effect of VOD bottom blowing location and blowing rate on mixing time of molten steel was studied by a water model corresponding to 1/9 volume of the 75 t ladle with oval cross section at Taiyuan Steel.The test results showed that the available blowing rate for model was 1.1~1.3 m³/h coresponding to flowing rate 350~460 L/min in VOD refining of 75 t molten steel; the location of single blowing brick at bottom was nearer to ladle center the mixing time was shorter; and the mixing time was obviously shorter as bottom blowing with 2 or 3 blowing bricks but there were optimum distribution locations af bottom bricks. There were optimurn matching of top blowing rate and bottom blowing rate and coresponding location during top-bottom blowing to get better effect.

Key words: VOD Refining, Water Mold, Mixing Time

摘要: 通过相当于太钢75 t椭圆形钢包容量1/9的水模型,采用N2模拟底吹氩和顶吹氧试验,研究了VOD底吹位置和吹气量对钢液混匀时间的影响。试验结果表明,模型合理吹气量为1.1~1.3 m3/h,相当于75t钢水VOD处理的吹气量350~460 L/min;单底吹砖位置越靠近钢包中心,混匀时间越短;用双底吹砖或三底吹砖吹气时,混匀时间明显缩短,但存在最佳底砖分布位置。顶底复吹时,为取得较好的效果,亦存在顶吹-底吹气量的最佳配合及相应的有利位置。