ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2006, Vol. 27 ›› Issue (3): 1-4.

    Next Articles

Scrap Steel-Electric Arc Furnace Steelmaking Flow Sheet and Recycle Economy

Li  Shiqi1, Zhang  Handong1,2,Chen  Yu1,Hao    Jingwei1   

  1. 1 School of Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 The People's Coverument of Xinjiang Bazhou,Kuerle 841000
  • Received:2005-12-20 Online:2006-05-08 Published:2023-03-09

废钢-电弧炉炼钢流程和循环经济

李士琦1,张汉东1,2,陈煜1,郝经伟1   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2新疆巴州人民政府,库尔勒841000
  • 作者简介:李士琦(1942-),男,首席教授,博士生导师,研究领域:冶 金技术和工艺。

Abstract: The development of are furnace steel in China and world as well as the resource and energy characteristics for scrap stcel-electric are furnace steelmaking flow sheet are analyzed,it is obtained that this flow sheet is beneficial to recycle economy and environmental protection.The ratio of arc furnace steel output to total output of steel produced in world  was 33. 1%,while the ratio of that in China was only 17.6%,according to domestic natural resource and energy resources  conditions,with improving energy structure and increasing scrap steel accumulated amount,the scrap steel-electric arc furnace steclmaking flow sheet has larger long-term developing space.

Key words:  , Electric , Are , Furace , Steelmaking, Serap , Steel, Recycle , Economy

摘要: 分析了世界和中国电炉钢的发展以及废钢-电弧炉炼钢流程的资源和能源特征,得出该流程是有利于循环经济和环境保护的生产流程。2003年世界电炉钢比达33.1%,我国电炉钢比仅为17.6%,根据我国的资源和能源条件,随着能源结构的改善和废钢积累量的增加,我国废钢-电弧炉炼钢流程有较大的长远发展空间。